Wire Accelerated Ageing
FOR: Wire $1,240Available wire accelerating ageing methods for standards including BSS7324 and samples such as Wire.
The test determines if the insulation of a wire has been converted to a thermoset material by polymer crosslinking. The test is performed for a short time period at a temperature much greater than the temperature rating of the insulation. To pass this test, the wire must withstand the bend and wet dielectric tests after the thermal exposure. This test may be applied to insulation materials which are not crosslinked as well. At the end of the test, we will report the results of the bend (LINK) and wet dielectric (LINK) tests.
Parameters that can be adjusted for this test include:
- Exposure Temperatures
- Exposure Duration(s)
- Number of Specimens
- Mounting Conditions of Specimens during Conditioning
Choose the exact method
Pricing and sample requirements vary by test method. Specific test requirements can be added on the request quote page. Final scope and pricing are confirmed by Lectromec usually within 24 hours.
Accelerated Aging
BSS7324 ยท 7.01
- Sample type
- Wire
- Specimens per test
- 1
- Length per test
- 24 in
Catalog data generated from Lectromec's controlled Box workbook, version
2655261484000. Internal and external lab-source information
is intentionally excluded from this public page.