Cable Wrinkle Test
FOR: Cable From $320; some methods require a quoteAvailable cable wrinkle test methods for standards including AS4373, AS6070 and samples such as Cable.
This test is used to evaluate the quality of insulation and its ability to withstand wrinkling. Wrinkles can occur to insulation when bent back and forth frequently, eventually causing the insulation to deteriorate.
The particular concern here is on tape wrapped insulations. During the fabrication process, an adhesive is used to hold the tape wrap layers together. If this adhesive is not prepared right in formulation or application, the tape wrap layers may separate during mechanical stressing. This layer separation can be often identified visually with the presence of wrinkles.
Choose the exact method
Pricing and sample requirements vary by test method. Specific test requirements can be added on the request quote page. Final scope and pricing are confirmed by Lectromec usually within 24 hours.
Wrinkle
AS4373 · 709
- Sample type
- Cable
- Specimens per test
- 1
- Length per test
- 12 in
Wrinkle
AS6070 · 5.4.3
- Sample type
- Cable
Catalog data generated from Lectromec's controlled Box workbook, version
2655261484000. Internal costing and supplier identities
are not published.