This test is used to evaluate the amount of weight lost, if any, from a wire specimen when exposed to temperature and vacuum for a period of several days.
Test specimens are placed in a chamber where they are subject to pressure of 33 mm Hg and the wire’s rated temperature for 384 hours (16 days). The weight of each sample is measured both before and after the exposure and any weight loss is reported.