Quantity discounts available.
The Nitric acid immersion test determines the ability of a wire’s insulation to resist breakdown in the presence of a strong acid. Test samples are submerged in red fuming nitric acid for a duration of 8 hours. Resistance to the acid is determined via a wet dielectric test – any dielectric breakdown is considered a test failure.