View Latest Blog Entries
Close
Categories
Testing & Assessment Certification Standard & Regulation Aging Wires & Systems Maintenance & Sustainment Protection & Prevention Management Conference & Report Research Miscellaneous Arcing
Popular Tags
Visual Inspection High Voltage AS50881 MIL-HDBK MIL-HDBK-525 FAR Electromagnetic Interference (EMI) AS4373 Maintenance FAR 25.1707 Wire System Circuit Protection
All Tags in Alphabetical Order
2021 25.1701 25.1703 abrasion AC 33.4-3 AC 43 Accelerated Aging accessibility ADMT Aging Systems AIR6808 AIR7502 Aircraft Power System aircraft safety Aircraft Service Life Extension Program (SLEP) altitude Aluminum arc damage Arc Damage Modeling Tool Arc Fault (AF) Arc Fault Circuit Breaker (AFCB) Arc Resistance Arc Track Resistance Arcing Arcing Damage AS22759 AS22759/87 AS23053 AS29606 AS4373 AS4373 Method 704 AS50881 AS5692 AS6019 AS6324 AS81824 AS83519 AS85049 AS85485 AS85485 Wire Standard ASTM B230 ASTM B355 ASTM B470 ASTM D150 ASTM D2671 ASTM D495 ASTM D8355 ASTM D876 ASTM F2639 ASTM F2696 ASTM F2799 ASTM F3230 ASTM F3309 ATSRAC Attenuation Automated Wire Testing System (AWTS) Automotive Avionics backshell batteries bend radius Bent Pin Analysis Best of Lectromec Best Practice bonding Cable Cable Bend cable testing Carbon Nanotube (CNT) Certification cfr 25.1717 Chafing Chemical Testing Circuit Breaker circuit design Circuit Protection cleaning clearance Coaxial cable cold bend collision comparative analysis Compliance Component Selection Condition Based Maintenance Conductor Conductor Testing conductors conduit Connector connector installation Connector rating connector selection connector testing connectors contacts Corona Corrosion Corrosion Preventing Compound (CPC) corrosion prevention Cracking creepage D-sub data analysis data cables degradat Degradation Delamination Derating design safety development diagnostic Dielectric breakdown dielectric constant Dimensional Life disinfectant Distributed Power System DO-160 dry arc dynamic cut through E-CFR electric aircraft Electrical Aircraft Electrical Component Electrical Power Electrical Testing Electrified Vehicles Electromagnetic Interference (EMI) Electromagnetic Vulnerability (EMV) Electrostatic Discharge EMC EMF EMI EN2235 EN3197 EN3475 EN6059 End of Service Life End of Year Energy Storage engines Environmental Environmental Cycling environmental stress ethernet eVTOL EWIS certification EWIS Component EWIS Design EWIS Failure EWIS sustainment EWIS Thermal Management EZAP FAA FAA AC 25.27 FAA AC 25.981-1C FAA Meeting failure conditions Failure Database Failure Modes and Effects Analysis (FMEA) FAQs FAR FAR 25.1703 FAR 25.1707 FAR 25.1709 Fault fault tree Filter Line Cable Fixturing Flammability fleet reliability Flex Testing fluid exposure Fluid Immersion Forced Hydrolysis fuel system fuel tank ignition Functional Hazard Assessment functional testing Fundamental Articles Fuse Future Tech galvanic corrosion Glycol Gold Gold plating Green Taxiing Grounding hand sanitizer handbook Harness Design harness protection hazard Hazard Analysis health monitoring heat shrink heat shrink tubing high current high Frequency high speed data cable High Voltage High Voltage Degradation HIRF History Hot Stamping Humidity Variation HV connector HV system ICAs IEC 60851 IEC60172 IEEE immersion insertion loss Inspection installation installation safety Instructions for Continued Airworthiness insulating material insulating tape Insulation insulation breakdown insulation resistance insulation testing interchangeability IPC-D-620 ISO 17025 Certified Lab ISO 9000 J1673 Kapton Laser Marking life limit life limited parts Life prediction life projection Lightning lightning protection liquid nitrogen lithium battery lunar Magnet wire maintainability Maintenance Maintenance costs Mandrel mean free path measurement mechanical stress Mechanical Testing MECSIP MIL-C-38999 MIL-C-85485 MIL-DTL-17 MIL-DTL-23053E MIL-DTL-3885G MIL-DTL-38999 MIL-E-25499 MIL-F-5372 MIL-HDBK MIL-HDBK-1646 MIL-HDBK-217 MIL-HDBK-454 MIL-HDBK-516 MIL-HDBK-522 MIL-HDBK-525 MIL-HDBK-683 MIL-STD-1353 MIL-STD-1560 MIL-STD-1798 MIL-STD-464 MIL-T-7928 MIL-T-7928/5 MIL-T-81490 MIL-W-22759/87 MIL-W-5088 MIL–STD–5088 Military 5088 modeling moon MS3320 NASA NEMA27500 Nickel nickel plating No Fault Found OEM off gassing Outgassing Over current Overheating of Wire Harness Parallel Arcing part selection Partial Discharge partial discharge at altitude Performance physical hazard assessment Physical Testing polyamide polyimdie Polyimide-PTFE Power over Ethernet power system Power systems predictive maintenance Presentation Preventative Maintenance Program Probability of Failure Product Quality PTFE pull through Radiation Red Plague Corrosion Reduction of Hazardous Substances (RoHS) regulations relays Reliability Research Resistance Revision C Rewiring Project Risk Assessment S&T Meeting SAE SAE Committee Sanitizing Fluids Scrape Abrasion Secondary Harness Protection separation separation distance Separation Requirements Series Arcing Service Life Extension Severe Wind and Moisture-Prone (SWAMP) Severity of Failure shelf life Shield Shielding Shrinkage signal signal cable Silver silver plated wire silver-plating skin depth skin effect Small aircraft smoke Solid State Circuit Breaker Space Certified Wires Splice standards Storage stored energy superconductor supportability Sustainment System Voltage Temperature Rating Temperature Variation Test methods Test Pricing Testing testing standard Thermal Circuit Breaker Thermal Endurance Thermal Index Thermal Runaway Thermal Shock Thermal Testing tin Tin plated conductors tin plating tin solder tin whiskering tin whiskers top 5 Transient Troubleshooting TWA800 UAVs UL94 USAF validation verification video Visual Inspection voltage voltage differential Voltage Tolerance volume resistivity vw-1 wet arc white paper whitelisting Winding wire Wire Ampacity Wire Bend Wire Certification Wire Comparison wire damage wire failure wire performance wire properties Wire System wire testing Wire Verification wiring components work unit code

Detailed Discussion of MIL-STD-1353 (Part 1): Tin Plating

Standard & Regulation

Key Takeaways
  • Despite environmental and operational limitations, tin remains common as a plating metal due to its conductivity, high solderability and low cost.
  • The MIL-STD-1353 standard forbids the use of pure tin to prevent dangerous tin whiskers from forming in electrical connectors.
  • Tin alloyed with lead is the most commonly used solder and is still applicable in low-frequency or appropriate circuit board applications.

Introduction

The mating of the electrical wiring interconnect system (EWIS) is a non-trivial task. Between the functional requirements (the correct number of pins, sizing of contacts, etc.), there are also the performance requirements (operational environment, corrosion resistance, impedance matching, etc.). This is then further complicated by installation requirements (sizing), maintenance requirements (mating/demating cycles), and regulatory requirements (limitations of materials that can be used). Obviously, adding a connector to a wire harness is not a five-second activity.

In a previous article, we looked at the MIL-STD-1353 standard on connector selection guidance in general terms. In this series of entries, we will examine a few of the specific requirements of the MIL-STD-1353 in a bit more detail. This article looks at the MIL-STD-1353 specific requirements for tin usage in aircraft connectors.

Acceptable Use of Tin in Aircraft Connectors

Tin is often considered a low-cost, highly conductive choice in material selection. In fact, it is the most common material used for soldering applications, when alloyed with Lead (Pb). On its own, however, tin can cause severe problems to an electrical system. The following examines some properties of tin, permissible applications, and limitations of its use in aircraft connectors.

The MIL-STD-1353 explicitly prohibits the use of pure tin in plating, underplating, or as a final finish either interior or exterior of the connector surface. This is due to pure tin’s tendency to produce “whiskers” which can be extremely dangerous for the aircraft.

Tin-Lead (Pb) solder, however, is recommended by the MIL-STD-1353 in solder and benign ground applications. Any tin solder used may have a maximum of 97% tin by mass and a minimum of 3% Pb by mass and adhere to the solderability testing standard MIL-STD-202 method 208.

Other limitations of tin-plated connectors include limiting its use in high frequency applications such as radio frequency circuits. Tin plated connectors should be limited to low-frequency applications to limit the signal attenuation (more conductive platings are recommended for high frequency signal transmission applications).

Tin whiskering

A tin whisker growing between a d-sub shell and connector pin. This can cause a short between the two conductive surfaces. Photo Credit to NASA Photo Gallery

Pure tin is known to produce “whiskers”; filament-like strands of tin protruding from the metallic surface over time.

Tin whiskers are conductive as they are an extension of the conductive tin surface; they grow gradually over time and have been observed to reach several mm in length. The conductive nature and significant length of these filaments introduces the opportunity for short circuiting or electrical arcing between components or systems. As discussed in several previous articles, a short circuit or electrical arc on an aircraft can cause very severe physical and functional damage.

In some cases, a whisker may cause a “metal vapor arc” in which the transfer of energy is so extreme that the solid metal whisker vaporizes into a plasma with a much higher conductivity. The increased conductivity allows for the arcing of much larger currents which will result in more severe damage.

Unfortunately, there is no confirmed agreement of a single consistent cause of tin whisker formation. Common consensus seems to lean toward the idea that whiskers are formed in conditions where the tin undergoes excess mechanical stress or compression. However, methods of mitigating the formation of tin whiskers can still be developed and implemented.

Whiskering is commonly mitigated by using tin/lead alloy solder (commonly 97% tin, 3% lead); in practice, the presence of lead inhibits the growth of whiskers. Though, with recent initiatives to reduce the use of toxic chemicals, such as lead, in commercial applications, alternate options of whisker mitigation may be researched and implemented (conformal – ceramic/ polymer coating, printed circuit boards with coating).

Environmental limitation

Of the plating options for connectors, Tin plated connectors have perhaps the most significant limitations.

  • Lowest max-temperature option. The relatively low melting point of tin makes it susceptible to intermetallic growth at significantly lower temperatures than other plating metals.
  • Lowest salt fog rating. The salt fog test is an evaluation of a plating material’s ability to withstand corrosive, humid conditions, namely salt-rich fog. A low rating in this respect implies poor performance of the material in particular climates.
  • Among the highest shell to shell conductivities. The shell-to-shell conductivity test measures the voltage drop across a connector when placed in a standard circuit. A larger value for this test means that there is a notably larger amount of energy dissipated via the connector.

Conclusion

Tin can be a particularly tricky metal to work with in aerospace and other applications, particularly when one considers its strict operational limits. Clearly, the opportunity for further research exists in the understanding of tin whisker formation. Until such research is readily available, however, means can be applied to mitigate this detrimental growth and tin may continue its use as an alloyed solder and a plating in low-frequency applications.

In the next article discussing MIL-STD-1353 requirements, we will continue the discussion of plating metals and examine nickel and gold – a very commonly paired combination.

Laura Wishart

Laura Wishart

Engineer, Lectromec

Laura has been with Lectromec since 2019 and has been a key contributor on projects involving testing of EWIS/fuel system failure modes, the impact of poor installation practices on EWIS longevity, and wire/cable certification testing. Her knowledge and attention to detail ensure consistent delivery of accurate test results from Lectromec’s lab.